So here are some images of one of the final molds. The form was milled using a 1/2" spherical bit. I pathed it to take one rough pass leaving 1/2" of material. However, on the final two passes, the speed of the mill proved to be a bit high. Much of the surface was frayed. Because this is more of an experiment, the accidental texture is a nice side effect which should interesting in the final cast.

The final mold.

Detail

Detail showing the obvious fraying

Detail